Plastic barrels sometimes appear brittle during use, and brittle plastic barrels are simply damaged, which is not conducive to long-term use. The brittleness of plastic barrels has a great relationship with the production mold, the selection of raw materials, the production machinery and the production process. Today, the manufacturer of plastic barrels will introduce to us how to avoid the brittleness of plastic barrels in terms of production process.
1. The temperature of the barrel and nozzle is too low and need to be adjusted higher. If the material is simply degraded, the temperature of the barrel and nozzle should be increased.
2. Decrease the screw pre-plastic back pressure and speed to make the material slightly looser and reduce the degradation of the plastic due to shearing overheating.
3. The mold temperature is too high and it is difficult to demold. Low mold temperature, premature cooling of the plastic, poor fusion of the weld seam, and simple cracking, especially for high-melting plastics such as polycarbonate.
4. The cavity and core must have proper demoulding inclination. When the core is difficult to demold, the temperature of the cavity should be increased to shorten the cooling time. When the cavity is difficult to take off, the temperature of the cavity should be lowered and the cooling time should be extended.